How to choose an induction heating frequency: reference depth, Curie point, case depth

Why frequency sets heating depth, how the Curie point changes it, and which frequency band suits a given case depth or bar diameter.

Updated 1 October 2026 · 6 min read

Frequency is the first number to fix when you specify an induction heater. It decides where the heat is generated in the part. Power and time then decide how hot that zone gets and how far the heat spreads by conduction. Get the frequency wrong and no amount of power will give you the right case depth or a uniform billet.

What frequency controls

The coil current induces eddy currents in the part. These currents are strongest at the surface and fall off quickly with depth. The depth where most of the heating happens is called the reference depth, or skin depth, δ:

δ = 503 · √(ρ / (μr · f))

  • δ is the reference depth in metres
  • ρ is the electrical resistivity of the part in Ω·m
  • μr is the relative magnetic permeability (no unit)
  • f is the frequency in Hz

About 86% of the induced power is generated inside one reference depth. So δ is a good first estimate of the heated layer before conduction spreads it.

Three things follow directly from the formula:

  1. Higher frequency gives a thinner heated layer. Doubling f reduces δ by a factor of √2, about 1.41.
  2. Higher resistivity gives a deeper layer.
  3. Higher permeability gives a thinner layer. This is why magnetic steel heats in a thin skin when it is cold.

A worked example on cold steel

Take a low-carbon steel at room temperature. Its resistivity is about 1.43 × 10⁻⁷ Ω·m. The relative permeability of magnetic materials used in induction heating is often between 100 and 500. Putting these values into the formula gives:

Frequency δ with μr = 100 δ with μr = 500
1 kHz 0.60 mm 0.27 mm
10 kHz 0.19 mm 0.085 mm
30 kHz 0.11 mm 0.049 mm
100 kHz 0.060 mm 0.027 mm

These depths look very small next to a 3 mm hardened case. The reason is the Curie point.

Why the depth changes above the Curie point

Iron loses its ferromagnetism at the Curie temperature, 770 °C for pure iron. Above that point the relative permeability of steel drops to 1. Resistivity also changes with temperature; for steel it rises as the part gets hotter. Both effects make δ larger.

For magnetic steels the reference depth can grow by as much as 20 times between cold and hot. In practice the part heats in two stages:

  • Below the Curie point the heat is concentrated in a very thin skin. The part heats fast and the coil couples well.
  • Above the Curie point the heated layer becomes much deeper. Heating slows, and the electrical load seen by the power supply changes.

Two practical points come out of this. First, when you choose a frequency for hardening, think about the hot depth, not the cold one. Induction hardening takes the surface to roughly 800–1000 °C, above the Curie point, so the hot δ sets the case. Second, the power supply must follow the load change during the cycle. JKZ controls use digital phase-locked loop tracking, so the output frequency follows the resonance of the coil and part as the part passes through the Curie point.

Through-heating: the diameter-to-depth ratio

For through-heating a bar or billet you want the current to flow in a ring near the surface, not across the whole section. If the frequency is too low, δ becomes large compared with the bar. Eddy currents from opposite sides then cancel each other and efficiency falls.

A common rule is that heating efficiency rises quickly as the ratio of bar diameter to reference depth increases, up to a ratio of about 4. Above that, a higher frequency gives little extra efficiency. So for through-heating, pick the lowest frequency that still gives a diameter at least about 4 times the hot reference depth. A higher frequency than needed only makes the surface run hotter than the core and stretches the soak time.

JKZ reference table

The table below is the guidance JKZ has published for choosing a frequency. It is a starting point. Material, part shape, coil design and cycle time all move the answer.

Job Requirement Suggested frequency
Surface hardening Case depth 0.8–1.2 mm 200–400 kHz
Surface hardening Case depth 1–2 mm 60–200 kHz
Surface hardening Case depth 2–4 mm 15–30 kHz
Through-heating (forging) Bar diameter 20–30 mm 15–30 kHz
Through-heating (forging) Bar diameter 30–50 mm 6–15 kHz
Through-heating (forging) Bar diameter 50–80 mm 2–5 kHz
Through-heating (forging) Bar diameter above 80 mm 2 kHz or lower
Melting Depends on metal and charge size 3–30 kHz
Brazing Depends on filler, joint and section 15–300 kHz

Notice the pattern. Deeper case or larger section means lower frequency. This is the formula at work.

How the bands map to JKZ series

Each JKZ series covers a band of frequency and power. The machine is tuned within its band to suit the coil and the part.

Series Frequency Power Fits these rows of the table
CX (high frequency) 50–120 kHz 15–60 kVA Shallow hardening (1–2 mm case), brazing, small parts
SWP-HT (digital) 30–60 kHz see note Between CX and SWS
SWS (ultrasonic frequency) 15–30 kHz 25–250 kW 2–4 mm case; through-heating 20–30 mm bars
SWP-MT (digital) 15–30 kHz see note Same band as SWS
SWP-LT (digital) 6–10 kHz see note Through-heating 30–50 mm bars
MFS (medium frequency) 1–8 kHz 120–600 kW Bars above 50 mm, deep heat treatment, melting

Note: the SWP digital platform reaches up to 800 kW from a single unit. Each SWP band has its own model list.

Some rows of the reference table fall outside these bands. Cases under about 1.2 mm call for 200–400 kHz, above the CX range. Very large bars may run best near the bottom of the MFS band. If your job sits at the edge of a band, tell us and we will look at the options with you.

Checklist before you ask for a quote

  • Material grade and its condition before heating
  • Part drawing with the zone to be heated marked
  • Required case depth and hardness, or the target temperature for through-heating
  • Required output in parts per hour or kg per hour
  • Whether parts are heated one at a time, by scanning, or continuously

Send us the drawing, material and target case depth, and our engineers will recommend a frequency and power.

Sources

  1. Wikipedia: Induction heating — Reference depth formula δ = 503·√(ρ/(μr·f)); 86% of the power inside δ; μr falls to 1 above the Curie temperature; depth can change by up to 20 times for magnetic steels (Zinn and Semiatin, Elements of Induction Heating, ASM, 1988); efficiency rises with diameter/depth up to about 4; permeability 100–500
  2. Wikipedia: Electrical resistivity and conductivity — Resistivity of carbon steel (1010) at 20 °C: 1.43 × 10⁻⁷ Ω·m
  3. Wikipedia: Curie temperature — Curie temperature of iron: 1043 K (770 °C)
  4. JKZ (old site): Induction Heating Frequency Selection — Reference table of frequency against hardening depth, bar diameter, melting and brazing
  5. JKZ (old site): Several commonly used tempering methods in induction quenching — Induction hardening raises the surface to 800–1000 °C in a few seconds
  6. JKZ (old site): The main components of induction heating machine — DSP control with digital phase-locked loop tracking
  7. JKZ product pages: CX, SWS, MFS and SWP series — Frequency and power ranges of each series; SWP up to 800 kW single unit (context.md §2)

Send us your part.

We reply within 1 working day.

Our timeUTC+8

[email protected]+86-28-84211110