Induction preheating and post-weld heat treatment of pipe: profile and measurement

Why pipe welds are preheated and stress relieved, the stages of a PWHT cycle, and how thermocouples and recorders control it with induction heating.

Updated 1 October 2026 · 6 min read

Welding puts a band of very hot metal next to cold metal. The weld and the heat-affected zone cool fast, harden, and lock in residual stress. On thick pipe, alloy steel and high-strength line pipe this can lead to cracking, sometimes hours after the weld is finished. Preheating before welding and heat treatment after welding are the two controls. Induction heating is one way to deliver both, on site or in the shop.

The welding procedure specification (WPS) and the code that applies to your project set the actual temperatures, times and rates. This guide explains what each stage does and how to measure it. It does not replace your procedure.

Why preheat

Preheating raises the temperature of the joint area before and during welding. It does three things:

  • Slows cooling after welding. A longer cooling time through the range from 800 °C to 500 °C gives diffusible hydrogen time to leave the weld metal. This reduces the risk of hydrogen cracking. It also gives a softer weld and heat-affected zone.
  • Reduces the temperature gradient across the joint, which lowers welding stress.
  • Reduces restraint in the joint, especially in fillet welds.

Good practice for local preheat:

  • Make the heated band wide. On either side of the joint it should reach at least three wall thicknesses out, with 100 mm as the minimum.
  • Keep the joint at or above the preheat temperature for the whole weld, not only at the start.
  • When joining two different steels, use the preheat temperature of the steel that needs the higher one.
  • Do not overshoot. Preheat far above what is needed can coarsen the grain next to the fusion line.

The preheat temperature itself comes from the material, thickness, restraint, welding process and the applicable standard. For critical work it is confirmed by crack testing.

Why post-weld heat treatment

PWHT heats the welded zone to a set temperature, holds it there, and cools it slowly. The purposes are:

  • Relax residual stress from welding
  • Bring down hardness in the weld metal and the heat-affected zone
  • Improve toughness of the joint

PWHT is common on pressure vessels, process pipe, and oil and gas lines, especially on thick walls and alloy steels.

The three stages of a PWHT cycle

A PWHT cycle has three controlled stages. The rates and times come from your procedure.

Stage What happens What to control
1. Controlled heating (ramp) The band is heated from below a set start temperature up to the holding temperature Maximum heating rate; temperature difference across the band
2. Holding (soak) The band is held at temperature Holding temperature range; holding time, often set by wall thickness
3. Controlled cooling The band cools at a limited rate down to a set temperature, then in still air under insulation Maximum cooling rate; temperature difference across the band

As a reference, the JKZ PWHT application note describes a typical cycle on its equipment: heating at about 100–150 °C per hour, up to a target temperature of 650–780 °C chosen for the material. These figures are an example. Your procedure and code govern.

Why limit the rates? A thick wall heats and cools from the outside. If the surface runs too far ahead of the bore, the temperature difference itself creates new stress. Slow ramps and controlled cooling keep the through-wall difference small.

How induction delivers the heat

For a pipe girth weld, the usual set-up is local external heating:

  1. Wrap insulation around the pipe over the heating band.
  2. Wind a flexible heating cable or copper tube over the insulation to form the coil. The cable length is chosen to suit the pipe size.
  3. Connect the cable to the induction power supply.
  4. Attach thermocouples and connect them to the controller and recorder.

The induced current heats the pipe wall directly. The coil itself stays cool. Insulation cuts losses by radiation and convection, and it protects the coil.

Two other PWHT methods exist: placing the whole part in a furnace, and firing burners inside an insulated vessel. Local induction heating suits long pipe runs and large structures that cannot go in a furnace.

For field preheating, air-cooled units with a flexible heating cable are common, because they need no water supply on site. Ask us which configuration suits your pipe sizes.

Measuring with thermocouples

The controller can only hold the profile it can see. Plan the thermocouples before you start.

  • Attach thermocouples directly to the pipe surface. Use the attachment method your procedure allows. A loose junction reads low and the controller will overheat the pipe.
  • Place a control thermocouple at the weld in the heated band.
  • Add monitoring thermocouples at the edges of the required uniform-temperature band. These show whether the band is wide enough.
  • On horizontal pipe, put thermocouples at the top and bottom. Hot air rises inside and outside the pipe, so the top often runs hotter.
  • On thick walls, think about the bore. The outside surface reads first. If your procedure needs a through-wall check, plan for it.
  • Check the compensating cable and connections before the cycle. Make sure each channel reads ambient temperature before power is applied.

The recorder keeps the time-temperature chart for every thermocouple. This chart is the record the inspector will ask for. In a closed-loop system the recorded temperature also feeds back to the power supply, which adjusts its output to follow the programmed profile.

Information to send for a PWHT or preheat system

  • Pipe material, outside diameter and wall thickness
  • Weld location and joint type
  • Required heating band width
  • Preheat temperature, or the PWHT holding temperature, holding time and ramp rates from your procedure
  • Site power supply and whether cooling water is available
  • Number of joints per day

Send us the drawing, material and the procedure requirements, and our engineers will recommend a frequency and power.

Sources

  1. JKZ application note: Induction Post Weld Heat Treatment (PWHT), PDF — Typical JKZ cycle: heating at 100–150 °C per hour to a target of 650–780 °C depending on the material; temperature recorder feeds the control system
  2. JKZ (old site): Induction post weld heat treatment (PWHT) — PWHT methods (furnace, internal firing, local external heating); heating band sized to the uniform zone required by ASME; data needed to select equipment
  3. JKZ (old site): Induction preheating machines — Preheating with a flexible heating cable wound on site, insulation over the coil
  4. JKZ (old site): Knowledge of the application of preheat treatment in welding — Effects of preheat; cooling time between 800 and 500 °C; local preheat width at least three times the thickness each side and not less than 100 mm; mixed-steel joints
  5. JKZ (old site): Application of PWHT post weld heat treatment — Purposes of PWHT: lower residual stress and hardness, better toughness

Send us your part.

We reply within 1 working day.

Our timeUTC+8